Send Message
Home ProductsMDI Based Polyurethane

Rebond Foam Making Liquid MDI Based Polyurethane

Certification
China Qingdao Exceed Fine Chemicals Co.,Ltd certification
China Qingdao Exceed Fine Chemicals Co.,Ltd certification
Customer Reviews
Exceed team is very professional and trustable. It is lucky to build business relationship with you.

—— Mr Nogarotto

Hope have a long relationship with you, I love China.

—— Mr Elmogy

Great thanks for help. Exceed is very Professional.

—— Mr Shirish

Thanks for your good after-sale service. Excellent training and technology support helps me a lot.

—— Modje

Good packaging, received product well.

—— Mr Nimit

Good partner

—— Mr Michele

I'm Online Chat Now

Rebond Foam Making Liquid MDI Based Polyurethane

Rebond Foam Making Liquid MDI Based Polyurethane
Rebond Foam Making Liquid MDI Based Polyurethane

Large Image :  Rebond Foam Making Liquid MDI Based Polyurethane

Product Details:
Place of Origin: China
Brand Name: EXCEEDCHEM
Certification: ISO9001:2008
Model Number: MDI based polyurethane preploymer Shore 85A
Payment & Shipping Terms:
Minimum Order Quantity: 1mt
Price: FOB Qingdao usd3.0/kg
Packaging Details: 20kg/drum; 200kg/drum
Delivery Time: 5-8 work days
Payment Terms: L/C, T/T
Supply Ability: 3000mt/month

Rebond Foam Making Liquid MDI Based Polyurethane

Description
Hardness: Shore A92 Appearance: Liquid
Base: MDI Based Prepolymer NCO%: 5.30-5.50
MOCA (%): 15.4 Packing: 20kg/drum; 200kg/drum
High Light:

Liquid MDI Based Polyurethane

,

Foam Making MDI Polyurethane

,

Rebond Foam MDI Polyurethane

MDI/Polyether Polyurethane Prepolymer Shore A92

1. Description

 

This is a MDI based polyether polyurethane prepolymer.

 

2. Characteristics

  • Water resistance
  • Low temperature resistance
  • Mold resistance

3. Applications

  • Roller
  • Plate and bar
  • Sealing ring
  • Castor

4. Typical properties

Type Appearance Viscosity(mPa.s/85℃) NCO% Packing(kg/drum)
  Liquid 400-420 5.30-5.50 20/200

 

5. Operating Procedure

 

First, the prepolymer should be preheated in 80-85℃. Second, after vacumming, the prepolymer is to be mixed with melting MOCA evenly. Third, with degassing, casting into mould, and vulcanization,and then demould. Lastly, the finished product should be post vulcanized.

 

6. Reaction parameters

 

Item MOCA (%) Gel time(min) Mixing temperature(℃) Post vulcanization(h)
Specification 15.4 3-4 80/120 10

 

 

7. Finished products properties

 

Item Hardness(Shore A) Tensile strength(MPa) Tear strength(KN/m) Rebounding(%)
Physical properties 92 30-33 75-78 31

 

 