logo
Send Message
Qingdao Exceed Fine Chemicals Co.,Ltd
products
products
Home > products > MDI Based Polyurethane > Shore A80 Odorless MDI Polyether Polyurethane

Shore A80 Odorless MDI Polyether Polyurethane

Product Details

Place of Origin: China

Brand Name: EXCEEDCHEM

Certification: ISO9001:2008

Model Number: MDI based polyurethane preploymer Shore 85A

Payment & Shipping Terms

Minimum Order Quantity: 1mt

Price: FOB Qingdao usd3.0/kg

Packaging Details: 20kg/drum; 200kg/drum

Delivery Time: 5-8 work days

Payment Terms: L/C, T/T

Supply Ability: 3000mt/month

Get Best Price
Highlight:

Odorless MDI Polyether Polyurethane

,

Shore A80 MDI Polyurethane

,

A80 MDI Polyether Polyurethane

Hardness:
Shore A80
NCO%:
5.00-4.20
MOCA (%):
11.5
Base:
MDI Based Prepolymer
Appearance:
Liquid
Packing:
20kg/drum; 200kg/drum
Hardness:
Shore A80
NCO%:
5.00-4.20
MOCA (%):
11.5
Base:
MDI Based Prepolymer
Appearance:
Liquid
Packing:
20kg/drum; 200kg/drum
Shore A80 Odorless MDI Polyether Polyurethane

MDI/Polyether Polyurethane Prepolymer Shore A80

1. Description

 

This is a MDI based polyether polyurethane prepolymer.

 

2. Characteristics

  • Water resistance
  • Low temperature resistance
  • Mold resistance

3. Applications

  • Roller
  • Plate and bar
  • Sealing ring

4. Typical properties

Type Appearance Viscosity(mPa.s/85℃) NCO% Packing(kg/drum)
  Liquid 210-230 5.00-4.20 20/200

 

5. Operating Procedure

 

First, the prepolymer should be preheated in 80-85℃. Second, after vacumming, the prepolymer is to be mixed with melting MOCA evenly. Third, with degassing, casting into mould, and vulcanization,and then demould. Lastly, the finished product should be post vulcanized.

 

6. Reaction parameters

 

Item MOCA (%) Gel time(min) Mixing temperature(℃) Post vulcanization(h)
Specification 11.5 4 80/120 10

 

 

7. Finished products properties

 

Item Hardness(Shore A) Tensile strength(MPa) Tear strength(KN/m) Rebounding(%)
Physical properties 80 16-18 40-45 32