logo
Qingdao Exceed Fine Chemicals Co.,Ltd
products
products
Home > products > Blend Polyol > MDI Based PTMEG System Microcellular Polyurethane for Automotive Suspension Jounce Bumper

MDI Based PTMEG System Microcellular Polyurethane for Automotive Suspension Jounce Bumper

Product Details

Payment & Shipping Terms

Get Best Price
Highlight:

Good hydrolysis resistance MDI Based PTMEG System

,

High strength Microcellular Polyurethane

,

Automotive Suspension Jounce Bumper Polyether Polyol

MDI Based PTMEG System Microcellular Polyurethane for Automotive Suspension Jounce Bumper
MDI Based PTMEG PU System For Microcellular Polyurethane (MC-PU) For Manufacturing Automotive Suspension Jounce Bumper
This MDI-based PTMEG system is specifically designed for manufacturing microcellular polyurethane automotive suspension jounce bumpers, offering excellent hydrolysis resistance and high strength characteristics.
Key Characteristics
  • Good hydrolysis resistance
  • High strength performance
Applications
  • Marine fender
  • Shock absorption mat
Typical Properties of PU Matrix
Product Name Appearance Viscosity (mPa*s/40℃) Density (g*cm⁻³/40℃) Package Specification (kg)
A-1170 Liquid 600~1000 1.01~1.02 190
B-6003 Yellowish transparent liquid 500~700 1.08~1.2 225
Materials Preheating Requirements
  • A-1170: Preheat at 60~70℃ for 8~12 hours
  • B-6003: Preheat at 60~70℃ for 8~12 hours
Typical Processing & Reaction Parameters
Test Item Parameter Value
A/B Raw Material Temperature (℃) 30~35 / 35~40
Mix Ratio (by weight) A + 40g XC-2 + H₂O : B = 100 : 103~105
Cream Time (s) 8~10
Foam Peak Temperature (℃) 60~70
Free Rise Density (g/cm³) 0.30~0.35
Mold Temperature (℃) 35~45
Demold Time (min) 7~9
Auxiliary Material Addition Dosage
  • XC-2: 2.85Kg ± 0.5Kg per 190kg A-1170
  • Deionized Water: 0.3Kg ± 0.1Kg per 190kg A-1170 (adjust according to actual production)
Overall Molded Physical Properties Range
Item Index Range
Molded Density (g/cm³) 0.50~0.70
Hardness (Shore A) 70~90
Tear strength (kN/m) 29.5~44.5
Tensile strength (MPa) 8.0~11.0
Elongation (%) 335~450
Physical Properties Before Hydrolysis Test

Test Specimen: 6mm thick sheet

Item Test Result
Density (g/cm³) 0.6
Hardness (Shore A) 80
Elongation (%) 350
Tear strength (kN/m) 37.8
Tensile strength (MPa) 8.3
Physical Properties After 7 Days Hydrolysis Aging

Test Specimen: 6mm thick sheet
Hydrolysis Test Condition: 80℃, 95% relative humidity

Item Test Result
Density (g/cm³) 0.6
Hardness (Shore A) 75
Elongation (%) 396
Tear strength (kN/m) 37.0
Tensile strength (MPa) 8.2
Physical Properties After 14 Days Hydrolysis Aging

Test Specimen: 6mm thick sheet

Item Test Result
Density (g/cm³) 0.6
Hardness (Shore A) 70
Elongation (%) 412
Tear strength (kN/m) 35.9
Tensile strength (MPa) 8.0
Shelf Life
Material Model Shelf Life
A-1170 6 Months
B-6003 6 Months
XC-2 6 Months
XC-100 6 Months
MDI Based PTMEG System technical diagram
Important Notes
  • All data listed in this document are for reference only
  • Final technical indicators shall be subject to actual production test results
  • Please contact our technical team if customized physical performance requirements are needed
Frequently Asked Questions
Q: What is the MDI Based PTMEG System and what makes it suitable for automotive jounce bumpers?
A: This is a two-component microcellular polyurethane (MC-PU) system consisting of A-1170 (polyol side) and B-6003 (isocyanate side), based on MDI and PTMEG chemistry. The PTMEG polyether backbone provides exceptional hydrolysis resistance, while the MDI-based isocyanate delivers high mechanical strength and durability. These properties are critical for automotive suspension jounce bumpers, which must withstand repeated compression, exposure to moisture, road salts, and temperature extremes throughout the vehicle's service life.
Q: What are the preheating and processing temperature requirements for this system?
A: Both A-1170 and B-6003 must be preheated at 60-70°C for 8-12 hours before processing. During molding, the recommended raw material temperatures are 30-35°C for A-1170 and 35-40°C for B-6003. The mold temperature should be maintained at 35-45°C. The cream time is 8-10 seconds and foam peak temperature reaches 60-70°C. Demolding can be done in 7-9 minutes, enabling efficient production cycles.
Q: How does the system perform in hydrolysis resistance testing?
A: The system demonstrates excellent hydrolysis resistance. After 7 days of accelerated aging at 80°C and 95% relative humidity, the elastomer retains hardness of Shore A 75 (vs. 80 initial), tensile strength of 8.2 MPa (vs. 8.3 MPa), and tear strength of 37.0 kN/m (vs. 37.8 kN/m). Even after 14 days under the same conditions, key properties remain stable with tear strength at 35.9 kN/m and tensile strength at 8.0 MPa. Notably, elongation actually increases slightly during hydrolysis aging, indicating good structural integrity retention.
Q: What is the mix ratio and how should auxiliary additives be incorporated?
A: The recommended mix ratio by weight is A + XC-2 + H₂O : B = 100 : 103~105. For each 190kg of A-1170, add 2.85 ± 0.5 kg of XC-2 and 0.3 ± 0.1 kg of deionized water. The water amount should be fine-tuned based on actual production conditions to achieve the target free rise density of 0.30-0.35 g/cm³ and molded density of 0.50-0.70 g/cm³. All components have a shelf life of 6 months when stored properly.