Product Details:
|
NCO%: | 3.50-3.70 | MOCA%: | 10 |
---|---|---|---|
Hardness: | Shore A85 | Base: | TDI-100/PTMG |
Color: | Colorless Liquid | ||
High Light: | Shore A85 PTMG Polyurethane Prepolymer,Polyurethane Prepolymer Colorless Liquid,PTMG Colorless Liquid |
TDI-100/PTMG Polyurethane Prepolymer Shore A85
1. Description
This is a TDI-100 based PTMG polyurethane prepolymer.
2. Characteristics
3. Applications
4. Typical properties
Type | Appearance | Viscosity(mPa.s/85℃) | NCO% | Packing(kg/drum) |
Solid | 1200-1300 | 3.50-3.70 | 20/200 |
5. Operating Procedure
First, the prepolymer should be preheated in 80-85℃. Second, after vacumming, the prepolymer is to be mixed with melting MOCA evenly. Third, with degassing, casting into mould, and vulcanization,and then demould. Lastly, the finished product should be post vulcanized.
6. Reaction parameters
Item | MOCA (%) | Gel time(min) | Mixing temperature(℃) | Post vulcanization(h) |
Specification | 10 | 11-12 | 85/120 | 10 |
7. Finished products properties
Item | Hardness(Shore A) | Tensile strength(MPa) | Tear strength(KN/m) | Rebounding(%) |
Physical properties | 85 | 26-27 | 60-65 | 61 |
Contact Person: Louis.liu