Send Message
Home ProductsTDI Based Polyurethane

Machine Parts Polyester Based Polyurethane Shore A80

Certification
China Qingdao Exceed Fine Chemicals Co.,Ltd certification
China Qingdao Exceed Fine Chemicals Co.,Ltd certification
Customer Reviews
Exceed team is very professional and trustable. It is lucky to build business relationship with you.

—— Mr Nogarotto

Hope have a long relationship with you, I love China.

—— Mr Elmogy

Great thanks for help. Exceed is very Professional.

—— Mr Shirish

Thanks for your good after-sale service. Excellent training and technology support helps me a lot.

—— Modje

Good packaging, received product well.

—— Mr Nimit

Good partner

—— Mr Michele

I'm Online Chat Now

Machine Parts Polyester Based Polyurethane Shore A80

Machine Parts Polyester Based Polyurethane Shore A80
Machine Parts Polyester Based Polyurethane Shore A80

Large Image :  Machine Parts Polyester Based Polyurethane Shore A80

Product Details:
Place of Origin: China
Brand Name: EXCEEDCHEM
Certification: ISO9001:2008
Model Number: TDI-100/Polyester Polyurethane Prepolymer Shore A80
Payment & Shipping Terms:
Minimum Order Quantity: 1mt
Price: FOB Qingdao usd3.0/kg
Packaging Details: 20kg/drum; 200kg/drum
Delivery Time: 5-8 work days
Payment Terms: L/C, T/T
Supply Ability: 3000mt/month

Machine Parts Polyester Based Polyurethane Shore A80

Description
NCO%: 3.00-3.20 MOCA%: 8.7
Hardness: Shore A80 Base: TDI-100/Polyester
Color: Colorless Liquid
High Light:

Machine Polyester Based Polyurethane

,

Machine Parts Polyester Polyurethane

,

Shore A80 Polyester Based Polyurethane

TDI-100/Polyester Polyurethane Prepolymer Shore A80

1. Description

 

This is a TDI-100 based Polyester polyurethane prepolymer.

 

2. Characteristics

  • High oil resistance
  • Abrasive resistance
  • Good michanical performance

3. Applications

  • Sieve plate
  • Machine parts
  • Sealing ring
  • Roller

4. Typical properties

Type Appearance Viscosity(mPa.s/85℃) NCO% Packing(kg/drum)
  Solid 2200-2400 3.00-3.20 20/200

 

5. Operating Procedure

 

First, the prepolymer should be preheated in 80-85℃. Second, after vacumming, the prepolymer is to be mixed with melting MOCA evenly. Third, with degassing, casting into mould, and vulcanization,and then demould. Lastly, the finished product should be post vulcanized.

 

6. Reaction parameters

 

Item MOCA (%) Gel time(min) Mixing temperature(℃) Post vulcanization(h)
Specification 8.7 12-13 85/120 10

 

 

7. Finished products properties

 

Item Hardness(Shore A) Tensile strength(MPa) Tear strength(KN/m) Rebounding(%)
Physical properties 80 45-47 65-70 38

 

 