Send Message
Qingdao Exceed Fine Chemicals Co.,Ltd
products
products
Home > products > TDI Based Polyurethane > Abrasive Resistance Shore A92 TDI Based Polyurethane For Sieve Plate

Abrasive Resistance Shore A92 TDI Based Polyurethane For Sieve Plate

Product Details

Place of Origin: China

Brand Name: EXCEEDCHEM

Certification: ISO9001:2008

Model Number: TDI-80/Polyester Polyurethane Prepolymer Shore A92

Payment & Shipping Terms

Minimum Order Quantity: 1mt

Price: FOB Qingdao usd3.0/kg

Packaging Details: 20kg/drum; 200kg/drum

Delivery Time: 5-8 work days

Payment Terms: L/C, T/T

Supply Ability: 3000mt/month

Get Best Price
Highlight:

Shore A92 TDI Polyurethane

,

Abrasive Resistance TDI Based Polyurethane

,

A92 TDI Based Polyurethane

NCO%:
4.30-4.50
MOCA%:
12.5
Hardness:
Shore A92
Raw Material:
TDI-80 Based
Appearance:
Solid
Application:
Sieve Plate
NCO%:
4.30-4.50
MOCA%:
12.5
Hardness:
Shore A92
Raw Material:
TDI-80 Based
Appearance:
Solid
Application:
Sieve Plate
Abrasive Resistance Shore A92 TDI Based Polyurethane For Sieve Plate

TDI-80/Polyester Polyurethane Prepolymer Shore A92

1. Description

 

This is a TDI-80 based Polyester polyurethane prepolymer.

 

2. Characteristics

 

(1) High oil resistance

(2) Abrasive resistance

(3) Good michanical performance

 

3. Applications

 

(1) Sieve plate

(2) Machine parts

(3) Sealing ring

(4)Roller

 

4. Typical properties

Type Appearance Viscosity(mPa.s/85℃) NCO% Packing(kg/drum)
  Solid 1400-1600 4.30-4.50 20 or 200

 

5. Operating Procedure

 

First, the prepolymer should be preheated in 80-85℃. Second, after vacumming, the prepolymer is to be mixed with melting MOCA evenly. Third, with degassing, casting into mould, and vulcanization,and then demould. Lastly, the finished product should be post vulcanized.

 

6. Reaction parameters

 

Item MOCA (%) Gel time(min) Mixing temperature(℃) Post vulcanization(h)
Specification 12.5 4-4.5 80/120 10

 

 

7. Finished products properties

 

Item Hardness(Shore A) Tensile strength(MPa) Tear strength(KN/m) Rebounding(%)
Physical properties 92 46-48 95-99 37